Dataset:
Tensile testing of ZK20 and ZEK200 alloys at room temperature - 10-3s-1

Tensile testing of as-cast and homogenized ZK20 (Mg-2Zn-0.5Zr wt.%) and ZEK200 (Mg-2Zn-0.5Zr-0.8RE wt.%) alloys at room temperature and strain-rate of 10-3 s-1