Uniaxial Tension Testing and FLC Testing at 200C and Three Strain Rates of Mg...
This dataset has no description
-
Rolled alloy 2+
Pictures showing Alloy 2+ rolled by about 70% at 275C using multiple passes -
Rolled alloy 2
Picture shows alloy 2 rolled by about 70% using multiple passes at 275C -
Rolled alloy 2
Pictures showing symmetric and asymmetric rolled Alloy 2 at 275C. Symmetric rolling resulted in cracking while asymmetric rolling did not. -
Pole figures from Alloy 2+ asymmetrically rolled at 135C ~32%
Inverse pole figures and pole figures from Alloy 2+ asymmetrically rolled at 135C ~32% -
Pole figures from Alloy 2+ asymmetrically rolled at 275C ~56%
Inverse pole figures and pole figures from Alloy 2+ asymmetrically rolled at 275C ~56% -
Pole figures from Alloy 2+ rolled symmetrically at 275C ~ 36%
Inverse Pole Figure of Alloy 2+ rolled symmetrically at 275C ~ 36% -
Pole figures from Alloy 2+ asymmetrically rolled at 275C ~36%
Shear ratio 1:1.2, reduction ~36% -
Formability of Alloy 2 as compared with other Mg alloys
Formability of Alloy 2 as compared with other Mg alloys -
Tensile properties of Alloy 2
Tensile properties of Alloy 2 -
Optical micrographs of Alloy 2 microstructure
Optical micrographs of Alloy 2 microstructure -
tensile curve of Alloy 2 plus T4 and peak-aged T6 condition
tensile curve of Alloy 2 plus T4 (480 °C) and peak-aged T6 (210 °C) condition -
Aging hardness response of Alloy 2 plus at 210 °C
Aging hardness curve of Alloy 2 plus at 210 °C -
Plot of I.E. at RT value of Alloy 2 plus as compared with other Mg alloys
Plot of I.E. at RT value of Alloy 2 plus as compared with other Mg alloys -
TEM/STEM characterization of Alloy 2 plus after T4
TEM/STEM characterization of Alloy 2 plus after T4 treatment. -
optical micrographs of Alloy 2 plus as-cast condition and after H480 homogeni...
characterization of Alloy 2 plus as-cast condition microstructure and microstructure after H480 homogenization -
EBSD characterization of Alloy 2 plus T4 condition
EBSD characterization of Alloy 2 plus T4 condition -
STEM-EDS characterization of Alloy 2 plus microstructure after T4 treatment
STEM-EDS characterization of Alloy 2 plus microstructure after T4 treatment -
STEM characterization of Alloy 2 plus microstructure after T6 treatment
STEM characterization of Alloy 2 plus microstructure after T6 treatment -
STEM characterization of Alloy 2 microstructure after annealing at 350C for 1...
STEM characterization of Alloy 2 microstructure after annealing at 350C for 10 minutes