Compression of Mg - 0.35Ca (wt.%) 300C - 10 -3, 10 -2, 10 -1 s-1
Compression testing was performed using an Instron 5582 universal testing system on cylindrical samples of Mg – 0.35Ca, measuring 16 mm in diameter and 24 mm in height... -
Compression of Mg - 0.35Ca (wt.%) 200C - 10 -3, 10 -2, 10 -1 s-1
Compression testing was performed using an Instron 5582 universal testing system on cylindrical samples of Mg – 0.35Ca, measuring 16 mm in diameter and 24 mm in height... -
Compression of Mg - 0.1Ca (wt.%) 250C - 10 -1, 10 -2, 10 -3 s-1
Compression stress - strain data of Mg - 0.1Ca (wt.%) compressed at 250C at 10 -3 , 10 -2 , 10 -1 s-1 .