Compression Mg - 0.35Ca (wt.%) at 250C - 10 - 3, 10 -2 and 10 -1
One of the factors related to solutes effect on texture is dynamic strain aging (DSA) which is observed as serrations in stress - strain curves during compression at high... -
Compression of Mg - 0.1Ca (wt.%) 300C - 10 -1, 10 -2, 10 -3 s-1
A key factor in the limited formability is the strong texture that develops during fabrication of wrought Mg alloys by rolling and extrusion. The predominance of the basal slip...