Rolled alloy 2+
Pictures showing Alloy 2+ rolled by about 70% at 275C using multiple passes -
Rolled alloy 2
Picture shows alloy 2 rolled by about 70% using multiple passes at 275C -
Rolled alloy 2
Pictures showing symmetric and asymmetric rolled Alloy 2 at 275C. Symmetric rolling resulted in cracking while asymmetric rolling did not. -
Pole figures from Alloy 2+ asymmetrically rolled at 135C ~32%
Inverse pole figures and pole figures from Alloy 2+ asymmetrically rolled at 135C ~32% -
Pole figures from Alloy 2+ asymmetrically rolled at 275C ~56%
Inverse pole figures and pole figures from Alloy 2+ asymmetrically rolled at 275C ~56% -
Pole figures from Alloy 2+ rolled symmetrically at 275C ~ 36%
Inverse Pole Figure of Alloy 2+ rolled symmetrically at 275C ~ 36% -
Pole figures from Alloy 2+ asymmetrically rolled at 275C ~36%
Shear ratio 1:1.2, reduction ~36%