Compression of Mg - 0.1Ca (wt.%) 250C - 10 -1, 10 -2, 10 -3 s-1
Compression stress - strain data of Mg - 0.1Ca (wt.%) compressed at 250C at 10 -3 , 10 -2 , 10 -1 s-1 . -
Compression of Mg - 0.1Ca (wt.%) 300C - 10 -1, 10 -2, 10 -3 s-1
A key factor in the limited formability is the strong texture that develops during fabrication of wrought Mg alloys by rolling and extrusion. The predominance of the basal slip...