Rolled alloy 2+
Pictures showing Alloy 2+ rolled by about 70% at 275C using multiple passes -
Rolled alloy 2
Picture shows alloy 2 rolled by about 70% using multiple passes at 275C -
Rolled alloy 2
Pictures showing symmetric and asymmetric rolled Alloy 2 at 275C. Symmetric rolling resulted in cracking while asymmetric rolling did not.