Compression testing of homogenized Experimental Alloy 1

Compression testing of two homogenized Experimental Alloy 1 samples was performed at room temperature (RT) at 10-3 s-1 on cylindrical samples (10 mm in diameter and 12 mm in height). Given the low mechanical strength and strong basal texture, this alloy was not investigated further for this research program.